Stainless Steel 347/347H Pajpijiet mingħajr saldaturi Gradi Ekwivalenti:
| STANDARD | WERKSTOFF NR. | UNS | JIS | GOST | MT |
| SS 347 | 1.4550 | S34700 | SUS 347 | 08Ch18N12B | X6CrNiNb18-10 |
| SS 347H | 1.4961 | S34709 | SUS 347H | - | X6CrNiNb18-12 |
SS 347 / 347H Pajpijiet Seamless Kompożizzjoni Kimika u
| Grad | C | Mn | Si | P | S | Cr | Cb | Ni | Fe |
| SS 347 | 0.08 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 20.00 | 10xC – 1.10 | 9.00 – 13.00 | 62.74 min |
| SS 347H | 0.04 – 0.10 | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 8xC – 1.10 | 9.0 -13.0 | 63.72 min |
Proprjetajiet mekkaniċi:
| Densità | Punt tat-tidwib | Qawwa tat-tensjoni | Qawwa tar-Rendiment (0.2%Offset) | Titwil |
| 8.0 g/ċm3 | 1454 grad (2650 grad F) | Psi – 75000, MPa – 515 | Psi – 30000, MPa – 205 | 35 % |
Benefiċċji ta' 347 347H Stainless Steel
Stress ogħla ta 'creep u proprjetajiet ta' qsim meta mqabbla ma '304
Ideali għal servizz ta 'temperatura għolja
Jegħleb it-tħassib dwar is-sensitizzazzjoni u l-korrużjoni intergranulari
Jista 'jintuża f'applikazzjonijiet ta' temperatura elevata għal applikazzjonijiet tal-Kodiċi tal-Boiler u tal-Bastimenti tal-Pressjoni ASME
Minħabba l-istabbilizzazzjoni il-materjal joffri reżistenza ġenerali aħjar għall-korrużjoni meta mqabbel ma '304/304L
Proprjetajiet mekkaniċi eċċellenti
Verżjoni b'karbonju għoli (347H) hija wkoll disponibbli
It-tags Popolari: azzar li ma jissaddadx 347/347h pajpijiet mingħajr saldatura gradi ekwivalenti, iċ-Ċina stainless steel 347/347h pajpijiet mingħajr saldatura gradi ekwivalenti manifatturi, fornituri, fabbrika